Effect of Petrolatum Tape Cover on the Hydrogen Permeation of AISI4135 Steel under Marine Splash Zone Conditions
Qu, Wenjuan1,2; Huang, Yanliang1; Yu, Xiuming1,2; Zheng, Min1,2; Lu, Dongzhu1
2015-07-01
发表期刊INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE
卷号10期号:7页码:5892-5904
文章类型Article
摘要Influence of petrolatum tape cover (PTC) technology on the hydrogen permeation behavior of AISI4135 steel has been measured by electrochemical method under simulated splash zone conditions. The hydrogen permeation current of under PTC protection decreased dramatically compared with that without PTC protection. Moreover, the hydrogen permeation current has no significant change when the specimen surface was coated by petrolatum anti-corrosion grease and covered by petrolatum anti-corrosion tape. The PTC technology can provide better protective role for none corroded specimens. The resistances to corrosion were high after prolonged corrosion cycles, when the specimen surfaces were coated by petrolatum anti-corrosion grease and covered by petrolatum anti-corrosion tape.
关键词Hydrogen Permeation Petrolatum Coating Marine Splash Zone
收录类别SCI
语种英语
WOS记录号WOS:000359199100054
引用统计
被引频次:3[WOS]   [WOS记录]     [WOS相关记录]
文献类型期刊论文
条目标识符http://ir.qdio.ac.cn/handle/337002/49789
专题海洋环境腐蚀与生物污损重点实验室
作者单位1.Chinese Acad Sci, Inst Oceanol, Key Lab Marine Environm Corros & Biofouling, Qingdao 266071, Peoples R China
2.Univ Chinese Acad Sci, Beijing 100049, Peoples R China
第一作者单位中国科学院海洋研究所
推荐引用方式
GB/T 7714
Qu, Wenjuan,Huang, Yanliang,Yu, Xiuming,et al. Effect of Petrolatum Tape Cover on the Hydrogen Permeation of AISI4135 Steel under Marine Splash Zone Conditions[J]. INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE,2015,10(7):5892-5904.
APA Qu, Wenjuan,Huang, Yanliang,Yu, Xiuming,Zheng, Min,&Lu, Dongzhu.(2015).Effect of Petrolatum Tape Cover on the Hydrogen Permeation of AISI4135 Steel under Marine Splash Zone Conditions.INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE,10(7),5892-5904.
MLA Qu, Wenjuan,et al."Effect of Petrolatum Tape Cover on the Hydrogen Permeation of AISI4135 Steel under Marine Splash Zone Conditions".INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE 10.7(2015):5892-5904.
条目包含的文件
文件名称/大小 文献类型 版本类型 开放类型 使用许可
Effect of Petrolatum(1028KB)期刊论文出版稿限制开放CC BY-NC-SA浏览
个性服务
推荐该条目
保存到收藏夹
查看访问统计
导出为Endnote文件
谷歌学术
谷歌学术中相似的文章
[Qu, Wenjuan]的文章
[Huang, Yanliang]的文章
[Yu, Xiuming]的文章
百度学术
百度学术中相似的文章
[Qu, Wenjuan]的文章
[Huang, Yanliang]的文章
[Yu, Xiuming]的文章
必应学术
必应学术中相似的文章
[Qu, Wenjuan]的文章
[Huang, Yanliang]的文章
[Yu, Xiuming]的文章
相关权益政策
暂无数据
收藏/分享
文件名: Effect of Petrolatum Tape Cover on the Hydrogen Permeation of AISI4135 Steel under Marine Splash Zone Conditions.pdf
格式: Adobe PDF
所有评论 (0)
暂无评论
 

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。